No Parameter UoM Method Spec Allowance
1 Grammage gsm ISO-536 75 GSM ±2.5
2 Tearing Strength ISO-1974
Machine Direction (MD) mN 1.030 min
Cross Direction (CD) mN 1.123 min
3 Stretch of Rupture ISO-1924-3
Machine Direction (MD) % 6,2 min
Cross Direction (CD) % 6 min
4 Tensile Energy Absorption (TEA) ISO-1924-3
Machine Direction (MD) J/m2 225 min
Cross Direction (CD) J/m2 225 min
5 Tensile Energy Absorption (TEA) Index ISO-1924-3
Machine Direction (MD) J/g 3 min
Cross Direction (CD) J/g 3 min
6 Air permeability (Gurley Number) s/100ml ISO-5636-5 8 max
7 Diameter Core mm Manual 76
8 Diameter Roll mm Manual 1.200 +5%
9 Sheet width mm Manual 1.010 +0,4%
10 Colour Visual Beige
|