Pulping Process: Kraft Bleaching Process: ECF Wood Species: Southern Pine Typical Properties Average Fiber Length Length Weighted (mm): 2.7 Weight Weighted (mm): 3.4 Basis Weight (g/m2): 685 ... View details

Get free quotes from
1 product from 1 company in 1 country
Pulping Process: Kraft Bleaching Process: ECF Wood Species: Southern Pine Typical Properties Average Fiber Length Length Weighted (mm): 2.7 Weight Weighted (mm): 3.4 Basis Weight (g/m2): 685 ... View details
Country
State
City
Payment Options | T/T |
Pulping Process: Kraft Bleaching Process: ECF Wood Species: Southern Pine Typical Properties Average Fiber Length Length Weighted (mm): 2.7 Weight Weighted (mm): 3.4 Basis Weight (g/m2): 685 ...